(In this model the shore 40 mix of tangoblack+ and verowhite+ was next to the verowhite+. This mixture does not attach sufficiently to the verowhite that a simple cut can be used. Actually the tip consist of the softest "hard" mix of tangoblack+ and vero)
(In this model the shore 40 mix of tangoblack+ and verowhite+ was next to the verowhite+. This mixture does not attach sufficiently to the verowhite that a simple cut can be used. Actually the tip consist of the softest "hard" mix of tangoblack+ and vero)
Current revision as of 09:15, 19 September 2011
In this model the shore 40 mix of tangoblack+ and verowhite+ was next to the verowhite+. This mixture does not attach sufficiently to the verowhite that a simple cut can be used.
Actually the tip consist of the softest "hard" mix of tangoblack+ and verowhite+ coated with 2mm shore 40 mix. The tip is about as flexible as it should, but the connection between shore 40 and vw+ is simply not good enough.
A better approach would have been to make shells with a more complex cut (3 shells more entangled) and avoided the use of coating on the tip.
File history
Click on a date/time to view the file as it appeared at that time.
(Latest | Earliest) View (newer 50) (older 50) (20 | 50 | 100 | 250 | 500)Date/Time | Thumbnail | Dimensions | User | Comment | |
---|---|---|---|---|---|
current | 09:15, 19 September 2011 | 400×300 (54 KB) | Yngveha (Talk | contribs) | (In this model the shore 40 mix of tangoblack+ and verowhite+ was next to the verowhite+. This mixture does not attach sufficiently to the verowhite that a simple cut can be used. Actually the tip consist of the softest "hard" mix of tangoblack+ and vero) |
- Edit this file using an external application (See the setup instructions for more information)
File links
The following page links to this file: